Specifications
Item | Specification |
Appearance | White crystal powder |
Initial Melting PointºC≥ | 60.0 |
Loss on Drying%≤ | 0.50 |
Ash%≤ | 0.30 |
Residue on 250μm Sieve,%≤ | 0.50 |
Physical property |
Density at 20ºC(kg/m³) | 1060 |
Bulk density(kg/m³) | 360-390 |